FERRIT-PM-KERN

|
MODELL |
G.W |
GRÖSSE (mm) |
||||||
|
A |
B |
C |
D |
E |
F |
|||
|
PM50 |
172 |
49.1±0.9 |
39.6±0.6 |
19.7±0.3 |
5.5±0.1 |
13.4±0.2 |
19.9±0.2 |
|
|
PM74 |
586 |
74.0 |
+0 |
57.0Minuten |
29.0±1.0 |
5.4±0.3 |
20.5±0.4 |
29.5±0.3 |
|
-3 |
||||||||
|
PM87 |
860 |
87.0 |
+2 |
66,5 Minuten |
31.7±1.5 |
8.5±0.4 |
24.2±0.4 |
35.0±0.4 |
|
-3 |
||||||||
|
MODELL |
PARAMETER |
AL±25 %(nH/N^2) |
N.W(g) |
|||
|
C1 mm-1 |
Lemm |
Ähm2 |
Vemm3 |
ZP40 |
||
|
PM50 |
0.227 |
84 |
370.0 |
31000.0 |
7700 |
153 |
|
PM74 |
0.162 |
128 |
790.0 |
101000.0 |
10000 |
515 |
|
PM87 |
0.161 |
146 |
910.0 |
133000.0 |
13000 |
770 |
Beliebte label: Ferrit-PM-Kern, China Ferrit-PM-Kern Hersteller, Lieferanten, Fabrik
You May Also Like
Anfrage senden