FERRIT-EPC-KERNE

|
MODELL |
G.W |
GRÖSSE (mm) |
|||||||
|
A |
Bmin |
C |
D |
E |
F |
G |
Hmin |
||
|
EPC13 |
2.5 |
13.3±0.3 |
8.3 |
5.6±0.2 |
4.6±0.2 |
4.5±0.2 |
6.6±0.2 |
2.1±0.1 |
10.5 |
|
EPC17.8 |
5.6 |
17.8±0.4 |
11.5 |
7.4±0.2 |
6.0±0.2 |
6.0±0.2 |
8.7±0.2 |
2.8±0.1 |
14.3 |
|
EPC34 |
62 |
34.0±0.5 |
19.7 |
14.5±0.2 |
14.5±0.2 |
16.4±0.2 |
20.9±0.2 |
9.1±0.2 |
24.8 |
|
EPC39 |
78 |
39.0±0.7 |
24.7 |
17.6±0.3 |
15.5±0.2 |
14.1±0.3 |
19.6±0.2 |
9.7±0.1 |
30.5 |
|
EPC41 |
108 |
41.0±0.6 |
23.6 |
18.5±0.2 |
16.5±0.2 |
18.9±0.2 |
24.5±0.2 |
11.0±0.2 |
28.8 |
|
MODELL |
PARAMETER |
AL±25 %(nH/N^2) |
N.W(g) |
|||
|
C1 mm-1 |
Lemm |
Ämm2 |
Vemm3 |
ZP40 |
||
|
EPC13 |
2.46 |
30.6 |
12.5 |
382.0 |
870 |
2.1 |
|
EPC17.8 |
1.77 |
40.2 |
22.7 |
917.0 |
1200 |
4.5 |
|
EPC34 |
0.73 |
89.6 |
122.6 |
10985.0 |
3200 |
56.0 |
|
EPC39 |
0.60 |
87.95 |
147.0 |
12960.0 |
3700 |
70.5 |
|
EPC41 |
0.57 |
104.1 |
183.2 |
19064.0 |
4100 |
97.0 |